The company provides a contract surface chemical analysis and depth profiling service. Using a range of techniques (including SIMS, Auger, LIMA and AFM), our analysts can help with issues such as dopant and contaminant profiling, failure analysis, delamination, adhesion and wire bonding failure. We have experience in analysing a wide range of technologies, including thin-film devices and read-write heads.